katangian | kundisyon | petsa | yunit | |
Mga pagtutukoy ng optical | ||||
Koepisyent ng pagpapalambing | 1310nm1383nm1550nm1625nm | <0.35≤0.34≤0.21≤0.24 | dB/kmdB/kmdB/km dB/km | |
Attenuation vs.Wavelength | @1310nm@1550nm | 1285~1330nm1525~1575nm | ≤0.04≤0.03 | dB/kmdB/km |
Wavelenth Dispersion | 1285-1340nm1550nm1625nm | ≥-3.5 ≤3.5≤18≤22 | ps / (nm·km)ps / (nm·km)ps / (nm·km) | |
Zero-dispersion na wavelength | 1300~1324 | nm | ||
Zero-dispersion slope | ≤0.092 | ps/(nm2·km) | ||
Polarization Mode Dispersion PMDSingle fiber maximal valueFiber link value (M=20,Q=0.01%) | ≤0.20≤0.10 | ps/√kmps/√km | ||
cable cuoff wavelength | ≤1260 | nm | ||
Mode field diameter MFD | 1310nm | 9.2±0.4 | μm | |
Effective Group Index of Refraction Neff | 1310nm1550nm | 1.46751.4681 | ||
Point discontinuity | 1550nm | ≤0.05 | dB | |
Pagganap ng mga sukat | ||||
Diametro ng cladding | 125±0.7 | μm | ||
Cladding Non-circularity | ≤0.5 | % | ||
Ang lapad ng panlabas na patong | 245±10 | μm | ||
Cladding/Coating Concentricity | ≤12.0 | μm | ||
Core/cladding concentricity | ≤0.5 | μm | ||
curvature (radius) | ≥4 | μm | ||
haba | 2.0~50.4 | km/reel | ||
Pagganap sa kapaligiran(1310nm/1550nm) | ||||
Mamasa init | 85 ℃, halumigmig≥85%, 30 araw | ≤0.05 | dB/km | |
Tuyong init | 85℃±2℃,30 araw | ≤0.05 | dB/km | |
Pagdepende sa Temperatura | -60℃ ~ +85℃, dalawang linggo | ≤0.05 | dB/km | |
Paglulubog sa tubig | 23℃±5C 30 araw | ≤0.05 | dB/km | |
Pagganap ng mekanikal | ||||
Antas ng pagsubok ng patunay | >0.69 | GPa | ||
Macrobend loss100 turnsφ60mm1 turnsφ32mm | 1625nm1550nm | ≤0.1≤0.05 | dBdB | |
Lakas ng strip | 1.0~5.0 | N | ||
Dynamic na parameter ng pagkapagod | ≥20 |